Lifting

 

 

Description

Shrivelling, swellings, wrinkles or folds of varying severity at the paint surface.

Cause

Non uniform drying within the paint film. This may result from:

  1. Excessive film thickness.
  2. Insufficient drying time between coats, forced drying, non uniform air temperature.
  3. Use of wrong or poor quality thinner.

 

Prevention

  1. Apply paint in thin, even coats.
  2. Allow sufficient drying time between coats, ensure correct, uniform drying temperature.
  3. Use only recommended thinner.

 

Rectification

Allow the film to harden thoroughly. If the defect is slight, flatten, compound and polish the affected area. In severe cases rub down to the substrate and repaint.

 

 

Other Defects:

Back

Site Cookies

This site uses cookies to ensure that it gives you the best experience on our website and for gathering information in accordance to our cookie policy. If you continue to use our website, we will assume that you consent to to receive the cookies, as explained in our cookie policy, unless you change your cookie settings